Find suppliers for this alloy
C19900
| Elements | ||
|---|---|---|
| Cu(1) | Ti | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
||
| Min (%) | 2.9 | |
| Max (%) | Rem | 3.5 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties