| Elements | |||
|---|---|---|---|
| Cu(1) | Fe | Ti | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||
| Min (%) | 0.17 | 2.9 | |
| Max (%) | Rem | 0.23 | 3.4 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Flat Products | Mill-hardened Temper, TM - Hard | TM04 |
141 Typ |
131 Typ |
16 Typ |
310 Typ |
| Mill-hardened Temper, TM - XHMS Spring | TM08 |
155 Typ |
145 Typ |
9 Typ |
340 Typ |
|
| Mill-hardened Temper, TM -XHM - Extra Hard | TM06 |
150 Typ |
138 Typ |
12 Typ |
330 Typ |
|
| Melting Point - Liquidus°F | 1931 |
|---|---|
| Melting Point - Solidus°F | 1769 |
| Densitylb/cu in. at 68°F | 0.311 |
| Specific Gravity | 8.7 |
| Electrical Conductivity% IACS at 68°F | 13 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 39 |
| Modulus of Elasticity in Tensionksi | 17400 |