C19940
| Elements | ||||
|---|---|---|---|---|
| Cu(1) | Fe | Al | Ti | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
||||
| Min (%) | 0.05 | 0.50 | 2.5 | |
| Max (%) | Rem | 0.20 | 1.5 | 3.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| Strip | Mill-hardened Temper - SHMS | TM10 |
152 Min 167 Typ 181 Max |
| Densitylb/cu in. at 68°F | .307 |
|---|---|
| Specific Gravity | 8.5 |
| Electrical Conductivity% IACS at 68°F | 12 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 35.2 |
| Modulus of Elasticity in Tensionksi | 18129 |
Fabrication Properties
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties