C19950
| Elements | ||
|---|---|---|
| Cu(1) | Ti | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
||
| Min (%) | 3.5 | |
| Max (%) | Rem | 4.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 3000 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Strip | Super Spring | H14 |
203 Min 218 Typ 232 Max |
202 Min 217 Typ 231 Max |
0.5 Typ |
475 Typ |
| Densitylb/cu in. at 68°F | 0.31 |
|---|---|
| Specific Gravity | 5.6 |
| Electrical Conductivity% IACS at 68°F | 8 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 22 |
| Modulus of Elasticity in Tensionksi | 19400 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Consumer | Camera Parts | ||
| Electrical | Conductors, Electrical | ||
| Springs |
Applicable Specifications
Corrosion Properties