Find suppliers for this alloy
C20500
| Elements | ||||
|---|---|---|---|---|
| Cu | Pb | Zn | Fe | |
| Min (%) | 97.0 | |||
| Max (%) | 98.0 | 0.02 | Rem | 0.05 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties