Find suppliers for this alloyC23400
Chemical Composition
Element
Cu(1)PbZnFe
(1) Cu + Sum of Named Elements 99.8% min.
Min (%)81.0
Max (%)84.00.05Rem0.05
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingGood
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingNot Recommended
Spot WeldFair
Seam WeldNot Recommended
Butt WeldGood
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedGood
Machinability Rating30
Common Fabrication Processes
  • Drawing
Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialWelded Wire, Filer MetalOtherBlended with C18900 to produce C22000
Applicable Specifications
Form System Standard Description
WireASTMB134/B134MBRASS WIRE
Corrosion Properties

No information available.