Find suppliers for this alloy
C25600
| Elements | ||||
|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | |
|
(1) Cu + Sum of Named Elements 99.7% min. |
||||
| Min (%) | 71.0 | |||
| Max (%) | 73.0 | 0.05 | Rem | 0.05 |
Mechanical Properties
| Melting Point - Liquidus°F | 1765 |
|---|---|
| Melting Point - Solidus°F | 1697 |
| Densitylb/cu in. at 68°F | 0.309 |
| Specific Gravity | 8.56 |
| Electrical Conductivity% IACS at 68°F | 36.5 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 72 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10.9 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 16000 |
| Modulus of Rigidityksi | 6000 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties