	| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | As | |
| (1) Cu + Sum of Named Elements  99.7% min. | |||||
| Min (%) | 68.5 | 0.02 | |||
| Max (%) | 71.5 | 0.05 | Rem | 0.05 | 0.08 | 
| Form | Temper | Temper Code | Tensile Strength (ksi) | YS-0.5% Ext (ksi) | Elongation (%) | Rockwell B scale | Rockwell F scale | Rockwell 30T scale | Shear Strength (ksi) | Fatigue Strength** (ksi) | Section Size (in) | Cold Work (%) | 
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | ||||||||||||
| Flat Products | 1/2 Hard | H02 | 62 Typ | 52 Typ | 25 Typ | 70 Typ | 65 Typ | 40 Typ | 18 Typ | 0.04 | ||
| 1/4 Hard | H01 | 54 Typ | 40 Typ | 43 Typ | 55 Typ | 54 Typ | 36 Typ | 0.04 | ||||
| Extra Hard | H06 | 86 Typ | 65 Typ | 5 Typ | 88 Typ | 76 Typ | 46 Typ | 0.04 | ||||
| Extra Spring | H10 | 99 Typ | 65 Typ | 3 Typ | 93 Typ | 78 Typ | 0.04 | |||||
| Hard | H04 | 76 Typ | 63 Typ | 8 Typ | 82 Typ | 73 Typ | 44 Typ | 21 Typ | 0.04 | |||
| Nominal Grain Size 0.015 mm | OS015 | 53 Typ | 22 Typ | 54 Typ | 78 Typ | 43 Typ | 35 Typ | 14 Typ | 0.04 | |||
| Nominal Grain Size 0.025 mm | OS025 | 51 Typ | 19 Typ | 55 Typ | 72 Typ | 36 Typ | 0.04 | |||||
| Nominal Grain Size 0.035 mm | OS035 | 49 Typ | 17 Typ | 57 Typ | 68 Typ | 31 Typ | 34 Typ | 14 Typ | 0.04 | |||
| Nominal Grain Size 0.050 mm | OS050 | 47 Typ | 15 Typ | 62 Typ | 64 Typ | 26 Typ | 0.04 | |||||
| Nominal Grain Size 0.070 mm | OS070 | 46 Typ | 14 Typ | 65 Typ | 58 Typ | 15 Typ | 32 Typ | 13 Typ | 0.04 | |||
| Nominal Grain Size 0.100 mm | OS100 | 44 Typ | 11 Typ | 66 Typ | 54 Typ | 11 Typ | 13 Typ | 0.04 | ||||
| Spring | H08 | 94 Typ | 65 Typ | 3 Typ | 91 Typ | 77 Typ | 48 Typ | 23 Typ | 0.04 | |||
| Rod | 1/2 Hard | H02 | 70 Typ | 52 Typ | 30 Typ | 80 Typ | 42 Typ | 22 Typ | 1 | 20 | ||
| 1/8 Hard | H00 | 55 Typ | 40 Typ | 48 Typ | 60 Typ | 36 Typ | 1 | 6 | ||||
| Nominal Grain Size 0.050 mm | OS050 | 48 Typ | 16 Typ | 65 Typ | 65 Typ | 34 Typ | 1 | |||||
| Tube | Nominal Grain Size 0.025 mm | OS025 | 52 Typ | 20 Typ | 55 Typ | 75 Typ | 40 Typ | |||||
| Nominal Grain Size 0.050 mm | OS050 | 47 Typ | 15 Typ | 65 Typ | 64 Typ | 26 Typ | ||||||
| Solution Heat Treated and Cold Worked: Hard | TD04 | 78 Typ | 64 Typ | 8 Typ | 82 Typ | 73 Typ | 35 | |||||
| Wire | 1/4 Hard | H01 | 70 Typ | 20 Typ | 0.08 | |||||||
| 1/8 Hard | H00 | 58 Typ | 35 Typ | 38 Typ | 0.08 | |||||||
| Extra Hard | H06 | 124 Typ | 4 Typ | 0.08 | ||||||||
| Nominal Grain Size 0.015 mm | OS015 | 54 Typ | 56 Typ | 0.08 | ||||||||
| Nominal Grain Size 0.025 mm | OS025 | 52 Typ | 58 Typ | 0.08 | ||||||||
| Nominal Grain Size 0.035 mm | OS035 | 50 Typ | 60 Typ | 34 Typ | 0.08 | |||||||
| Nominal Grain Size 0.050 mm | OS050 | 48 Typ | 64 Typ | 0.08 | ||||||||
| Spring | H08 | 130 Typ | 3 Typ | 60 Typ | 22 Typ | 0.08 | ||||||
| Melting Point - Liquidus°F | 1750 | 
|---|---|
| Melting Point - Solidus°F | 1680 | 
| Densitylb/cu in. at 68°F | 0.308 | 
| Specific Gravity | 8.53 | 
| Electrical Conductivity% IACS at 68°F | 28 | 
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 70 | 
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11.1 | 
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 | 
| Modulus of Elasticity in Tensionksi | 16000 | 
| Modulus of Rigidityksi | 6000 | 
| Technique | Suitability | 
|---|---|
| Soldering | Excellent | 
| Brazing | Excellent | 
| Oxyacetylene Welding | Good | 
| Gas Shielded Arc Welding | Fair | 
| Coated Metal Arc Welding | Not Recommended | 
| Spot Weld | Good | 
| Seam Weld | Not Recommended | 
| Butt Weld | Good | 
| Capacity for Being Cold Worked | Excellent | 
| Capacity for Being Hot Formed | Fair | 
							  Common Fabrication Processes
							  
							
| Treatment | Minimum* | Maximum* | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Annealing | 800 | 1400 | ||
| Hot Working Temperature | 1350 | 1550 | ||
| Product Category | Product | Reason Category | Reason | 
|---|---|---|---|
| Architecture | Grillwork | Appearance | Color | 
| Grillwork | Corrosion Resistance | Corrosion Resistance | |
| Grillwork | Corrosion Resistance | Corrosion Resistance to the Atmosphere | |
| Grillwork | Forming Characteristics | Formability | |
| Grillwork | Mechanical Properties | Moderate Strength | |
| Automotive | Auto Radiator Tube | Conductivity (Thermal) | Thermal Conductivity | 
| Auto Radiator Tube | Corrosion Resistance | Resistance to Corrosion - General and Pitting in Water Radiators | |
| Auto Radiator Tube | Solderability | Solderability | |
| Heater Cord | Corrosion Resistance | Corrosion Resistance | |
| Heater Cord | Forming Characteristics | Formability | |
| Heater Cord | Mechanical Properties | Moderate Strength | |
| Radiators | Corrosion Resistance | Corrosion Resistance | |
| Radiators | Corrosion Resistance | Corrosion Resistance to Chemicals | |
| Radiators | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Radiators | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Radiators | Forming Characteristics | Formability | |
| Radiators | Mechanical Properties | Moderate Strength | |
| Radiators | Solderability | Solderability | |
| Radiators | Welding Characteristics | Weldability | |
| Tanks | Corrosion Resistance | Corrosion Resistance | |
| Tanks | Corrosion Resistance | Corrosion Resistance to Chemicals | |
| Tanks | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Tanks | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Tanks | Forming Characteristics | Formability | |
| Tanks | Mechanical Properties | Moderate Strength | |
| Tanks | Solderability | Solderability | |
| Tanks | Welding Characteristics | Weldability | |
| Builders Hardware | Finish Hardware | Appearance | Color | 
| Finish Hardware | Corrosion Resistance | Corrosion Resistance | |
| Finish Hardware | Forming Characteristics | Formability | |
| Finish Hardware | Mechanical Properties | Moderate Strength | |
| Hinges | Corrosion Resistance | Corrosion Resistance | |
| Hinges | Forming Characteristics | Formability | |
| Hinges | Mechanical Properties | Moderate Strength | |
| Kick Plates | Appearance | Color | |
| Kick Plates | Corrosion Resistance | Corrosion Resistance | |
| Kick Plates | Forming Characteristics | Formability | |
| Kick Plates | Mechanical Properties | Moderate Strength | |
| Locks | Appearance | Color | |
| Locks | Corrosion Resistance | Corrosion Resistance | |
| Locks | Forming Characteristics | Formability | |
| Locks | Mechanical Properties | Moderate Strength | |
| Push Plates | Appearance | Color | |
| Push Plates | Corrosion Resistance | Corrosion Resistance | |
| Push Plates | Mechanical Properties | Moderate Strength | |
| Stencils | Appearance | Color | |
| Stencils | Corrosion Resistance | Corrosion Resistance | |
| Stencils | Mechanical Properties | Moderate Strength | |
| Electrical | Flashlight Shells | Appearance | Color | 
| Flashlight Shells | Corrosion Resistance | Corrosion Resistance | |
| Flashlight Shells | Forming Characteristics | Cold Workability | |
| Flashlight Shells | Forming Characteristics | Formability | |
| Flashlight Shells | Mechanical Properties | Moderate Strength | |
| Lamp Fixtures | Appearance | Appearance | |
| Lamp Fixtures | Appearance | Color | |
| Lamp Fixtures | Corrosion Resistance | Corrosion Resistance | |
| Lamp Fixtures | Forming Characteristics | Formability | |
| Lamp Fixtures | Mechanical Properties | Moderate Strength | |
| Reflectors | Appearance | Appearance | |
| Reflectors | Corrosion Resistance | Corrosion Resistance | |
| Reflectors | Forming Characteristics | Formability | |
| Reflectors | Mechanical Properties | Moderate Strength | |
| Screw Shells | Corrosion Resistance | Corrosion Resistance | |
| Screw Shells | Forming Characteristics | Cold Workability | |
| Screw Shells | Forming Characteristics | Formability | |
| Screw Shells | Mechanical Properties | Moderate Strength | |
| Socket Shells | Corrosion Resistance | Corrosion Resistance | |
| Socket Shells | Mechanical Properties | Moderate Strength | |
| Fasteners | Eyelets | Appearance | Color | 
| Eyelets | Corrosion Resistance | Corrosion Resistance | |
| Eyelets | Forming Characteristics | Formability | |
| Eyelets | Mechanical Properties | Moderate Strength | |
| Fasteners | Appearance | Color | |
| Fasteners | Corrosion Resistance | Corrosion Resistance | |
| Fasteners | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Fasteners | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Fasteners | Forming Characteristics | Formability | |
| Fasteners | Mechanical Properties | Moderate Strength | |
| Grommets | Appearance | Color | |
| Grommets | Corrosion Resistance | Corrosion Resistance | |
| Grommets | Forming Characteristics | Formability | |
| Grommets | Mechanical Properties | Moderate Strength | |
| Pins | Appearance | Color | |
| Pins | Corrosion Resistance | Corrosion Resistance | |
| Pins | Forming Characteristics | Formability | |
| Pins | Mechanical Properties | Moderate Strength | |
| Rivets | Appearance | Color | |
| Rivets | Corrosion Resistance | Corrosion Resistance | |
| Rivets | Corrosion Resistance | Corrosion Resistance to Chemicals | |
| Rivets | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Rivets | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Rivets | Forming Characteristics | Cold Workability | |
| Rivets | Forming Characteristics | Formability | |
| Rivets | Mechanical Properties | Moderate Strength | |
| Screws | Appearance | Color | |
| Screws | Corrosion Resistance | Corrosion Resistance | |
| Screws | Corrosion Resistance | Corrosion Resistance to Chemicals | |
| Screws | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Screws | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Screws | Forming Characteristics | Formability | |
| Screws | Mechanical Properties | Moderate Strength | |
| Industrial | Bead Chain | Appearance | Color | 
| Bead Chain | Corrosion Resistance | Corrosion Resistance | |
| Bead Chain | Forming Characteristics | Formability | |
| Bead Chain | Mechanical Properties | Moderate Strength | |
| Chain | Appearance | Color | |
| Chain | Corrosion Resistance | Corrosion Resistance | |
| Chain | Forming Characteristics | Formability | |
| Chain | Mechanical Properties | Moderate Strength | |
| Liners | Corrosion Resistance | Corrosion Resistance | |
| Liners | Corrosion Resistance | Corrosion Resistance to Chemicals | |
| Liners | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Liners | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Liners | Forming Characteristics | Cold Workability | |
| Liners | Forming Characteristics | Formability | |
| Liners | Mechanical Properties | Moderate Strength | |
| Liners | Solderability | Solderability | |
| Power Cylinders | Corrosion Resistance | Corrosion Resistance | |
| Power Cylinders | Corrosion Resistance | Corrosion Resistance to Chemicals | |
| Power Cylinders | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Power Cylinders | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Power Cylinders | Forming Characteristics | Cold Workability | |
| Power Cylinders | Forming Characteristics | Formability | |
| Power Cylinders | Mechanical Properties | Moderate Strength | |
| Pumps | Corrosion Resistance | Corrosion Resistance | |
| Pumps | Corrosion Resistance | Corrosion Resistance to Chemicals | |
| Pumps | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Pumps | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Pumps | Forming Characteristics | Formability | |
| Pumps | Mechanical Properties | Moderate Strength | |
| Springs | Corrosion Resistance | Corrosion Resistance | |
| Springs | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Springs | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Springs | Forming Characteristics | Formability | |
| Springs | Mechanical Properties | High Strength | |
| Ordnance | Ammunition Components | Corrosion Resistance | Corrosion Resistance | 
| Ammunition Components | Forming Characteristics | Formability | |
| Ammunition Components | Mechanical Properties | Moderate Strength | |
| Plumbing | Plumbing Accessories | Appearance | Color | 
| Plumbing Accessories | Corrosion Resistance | Corrosion Resistance | |
| Plumbing Accessories | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Plumbing Accessories | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Plumbing Accessories | Forming Characteristics | Formability | |
| Plumbing Accessories | Mechanical Properties | Moderate Strength | |
| Plumbing Brass Goods | Appearance | Color | |
| Plumbing Brass Goods | Corrosion Resistance | Corrosion Resistance | |
| Plumbing Brass Goods | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Plumbing Brass Goods | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Plumbing Brass Goods | Forming Characteristics | Formability | |
| Plumbing Brass Goods | Mechanical Properties | Moderate Strength | 
| Form | Specific Sub-Form | Application | System | Standard | Description | 
|---|---|---|---|---|---|
| Tube | Heat Exchanger | ASTM | B569 | BRASS STRIP IN NARROW WIDTHS AND LIGHT GAGE FOR HEAT EXCHANGER TUBING | 
								Corrosion Properties