Find suppliers for this alloy
C28320
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | B | C | Mn | S | Ti | Zr | |
|
(1) Cu + Sum of Named Elements 99.3% min. |
||||||||||
| Min (%) | 58.0 | 31.0 | 0.10 | |||||||
| Max (%) | 62.0 | 0.09 | 41.0 | 0.35 | 0.20 | 0.10 | 0.20 | 0.65 | 0.30 | 0.20 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties