C28330
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | B | C | Mn | S | Sb | Ti | Zr | |
|
(1) Cu + Sum of Named Elements 99.3% min. |
|||||||||||
| Min (%) | 58.0 | 31.0 | 0.10 | ||||||||
| Max (%) | 62.0 | 0.09 | 39.0 | 0.35 | 0.10 | 0.10 | 0.20 | 0.25 | 1.5 | 0.10 | 0.10 |
| Form | Temper | Temper Code | YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 3000 kg load | Ultimate Tensile Strength in Shear (ksi) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Rod | Hard | H04 | 1 Typ |
99 Typ |
110 Typ |
|
| Hard and Stress Relieved | HR04 | 26.5 Typ |
18 Typ |
65 Typ |
58 Typ |
|
| Melting Point - Liquidus°F | 1930 |
|---|---|
| Melting Point - Solidus°F | 1795 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 67 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11.4 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.096 |
| Magnetic Permeability | 1 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties