Find suppliers for this alloyC28330
Chemical Composition
Element
Cu(1)PbZnFeBCMnSSbTiZr
(1) Cu + Sum of Named Elements 99.3% min.
Min (%)58.031.00.10
Max (%)62.00.0939.00.350.100.100.200.251.50.100.10
Mechanical Properties*
Form
Temper
Temper Code
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 3000 kg load
Ultimate Tensile Strength in Shear
(ksi)
RodHardH04   Typ
1   Typ
99   Typ
110   Typ
Hard and Stress RelievedHR0426.5   Typ
18   Typ
65   Typ
58   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1930
Melting Point - Solidus°F1795
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F67
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)11.4
Specific Heat CapacityBtu/ lb /°F at 68°F0.096
Magnetic Permeability1
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.