C28550
Elements | ||||||||
---|---|---|---|---|---|---|---|---|
Cu(1) | Pb | Zn | Fe | P | Bi | C | Si | |
(1) Cu + Sum of Named Elements 99.5% min. |
||||||||
Min (%) | 57.0 | 0.20 | ||||||
Max (%) | 60.0 | 0.04 | Rem | 0.35 | 0.40 | 0.009 | 1.2 | 0.009 |
Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell B scale |
---|---|---|---|---|---|---|
* Measured at room temperature, 68°F (20°C). | ||||||
Rod, Bar & Forging | 1/4 Hard | H01 |
55 Min 59 Typ |
35 Min 40 Typ |
10 Min 20 Typ |
62 Typ |
Physical Properties
Technique | Suitability |
---|---|
Soldering | Excellent |
Brazing | Good |
Oxyacetylene Welding | Fair |
Gas Shielded Arc Welding | Fair |
Coated Metal Arc Welding | Not Recommended |
Spot Weld | Good |
Seam Weld | Not Recommended |
Butt Weld | Fair |
Capacity for Being Cold Worked | Poor |
Capacity for Being Hot Formed | Excellent |
Forgeability Rating | 90 |
Machinability Rating | 90 |