C28580
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Zn | Fe | Al | |
| Min (%) | 49.0 | ||||
| Max (%) | 52.0 | 0.50 | Rem | 0.10 | 0.10 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties