C35340
| Elements | ||||
|---|---|---|---|---|
| Cu | Pb | Zn | Fe | |
| Min (%) | 60.0 | 1.5 | 0.10 | |
| Max (%) | 63.0 | 2.5 | Rem | 0.30 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.306 |
|---|---|
| Specific Gravity | 8.47 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Strip | ASTM | B121/B121M | LEADED BRASS PLATE, SHEET, STRIP AND ROLLED BAR |
Corrosion Properties