Find suppliers for this alloy
C36300
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | P | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||
| Min (%) | 61.0 | 0.25 | 0.04 | ||
| Max (%) | 63.0 | 0.7 | Rem | 0.15 | 0.15 |
Mechanical Properties
| Melting Point - Liquidus°F | 1650 |
|---|---|
| Melting Point - Solidus°F | 1630 |
| Densitylb/cu in. at 68°F | 0.304 |
| Specific Gravity | 8.42 |
| Electrical Conductivity% IACS at 68°F | 26 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 51.5 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.088 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Fair |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Not Recommended |
| Spot Weld | Fair |
| Seam Weld | Not Recommended |
| Butt Weld | Fair |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Good |
| Machinability Rating | 80 |
Common Fabrication Processes
| Treatment | Minimum* | |||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Stress Relief | 500 | |||
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Rod, Bar & Shapes | ASTM | B981/B981M | LOW LEADED BRASS ROD, BAR AND SHAPES |
Corrosion Properties