Find suppliers for this alloyC36300
Chemical Composition
Element
Cu(1)PbZnFeP
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)61.00.250.04
Max (%)63.00.7Rem0.150.15
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Melting Point - Liquidus°F1650
Melting Point - Solidus°F1630
Densitylb/cu in. at 68°F0.304
Specific Gravity8.42
Electrical Conductivity% IACS at 68°F26
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F51.5
Specific Heat CapacityBtu/ lb /°F at 68°F0.088
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingGood
Oxyacetylene WeldingFair
Gas Shielded Arc WeldingFair
Coated Metal Arc WeldingNot Recommended
Spot WeldFair
Seam WeldNot Recommended
Butt WeldFair
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedGood
Machinability Rating80
Fabrication Process Properties

No fabrication process properties for this alloy

    
Thermal Properties
Treatment Value*
* Temperature is measured in Fahrenheit.
Stress Relief500
Typical Uses

No information available.

Applicable Specifications
Form System Standard Description
Rod, Bar & ShapesASTMB981/B981MLOW LEADED BRASS ROD, BAR AND SHAPES
Corrosion Properties