Find suppliers for this alloy
C37710
| Elements | ||||
|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
||||
| Min (%) | 56.5 | 1.0 | ||
| Max (%) | 60.0 | 3.0 | Rem | 0.30 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Consumer | Valve Bodies for Agricultural Spray Tanks | Appearance | Color |
| Valve Bodies for Agricultural Spray Tanks | Corrosion Resistance | Corrosion Resistance | |
| Valve Bodies for Agricultural Spray Tanks | Forging Characteristics | Forgability | |
| Valve Bodies for Agricultural Spray Tanks | Forging Characteristics | Hot Die forgability | |
| Valve Bodies for Agricultural Spray Tanks | Machining Characteristics | Machinability | |
| Valve Bodies for Scuba & Propane Spray Tanks | Corrosion Resistance | Corrosion Resistance | |
| Valve Bodies for Scuba & Propane Spray Tanks | Forging Characteristics | Hot Die forgability | |
| Valve Bodies for Scuba & Propane Spray Tanks | Machining Characteristics | Machinability |
Applicable Specifications
Corrosion Properties