C38510
| Elements | |||
|---|---|---|---|
| Cu | Pb | Zn | |
| Min (%) | 56.0 | 2.5 | |
| Max (%) | 60.0 | 4.5 | Rem |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties