Find suppliers for this alloy
C38590
| Elements | ||||
|---|---|---|---|---|
| Cu | Pb | Zn | Fe | |
| Min (%) | 56.5 | 2.0 | ||
| Max (%) | 60.0 | 3.5 | Rem | 0.35 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties