C38600
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Zn | Fe | Sb | |
| Min (%) | 56.0 | 2.5 | |||
| Max (%) | 59.0 | 3.5 | Rem | 0.35 | 0.02 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties