C40900
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | |
| Min (%) | 92.0 | 0.50 | |||
| Max (%) | 94.0 | 0.05 | 0.8 | Rem | 0.05 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties