C41110
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | |
|
(1) Cu + Sum of Named Elements 99.7% min. |
|||||
| Min (%) | 90.0 | 0.10 | |||
| Max (%) | 94.0 | 0.05 | 0.50 | Rem | 0.05 |