Elements | |||||
---|---|---|---|---|---|
Cu(1) | Pb | Sn | Zn | Fe | |
(1) Cu + Sum of Named Elements 99.7% min. |
|||||
Min (%) | 90.0 | 0.10 | |||
Max (%) | 94.0 | 0.05 | 0.50 | Rem | 0.05 |