Find suppliers for this alloy
C41900
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | |
| Min (%) | 89.0 | 4.5 | |||
| Max (%) | 92.0 | 0.10 | 5.5 | Rem | 0.05 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Strip | 1/4 Hard | H01 |
58 Typ |
46 Typ |
25 Typ |
| Annealed | O61 |
49 Typ |
19 Typ |
42 Typ |
|
| Hard | H04 |
82 Typ |
74 Typ |
4 Typ |
|
| Spring | H08 |
102 Typ |
80 Typ |
2 Typ |
|
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Connectors | Conductivity (Electrical) | Electrical Conductivity |
| Connectors | Conductivity (Thermal) | Thermal Conductivity | |
| Connectors | Mechanical Properties | Moderate Strength |
Applicable Specifications
Corrosion Properties