Find suppliers for this alloyC41900
Chemical Composition
Element
CuPbSnZnFe
Min (%)89.04.5
Max (%)92.00.105.5Rem0.05
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Strip1/4 HardH0158   Typ
46   Typ
25   Typ
AnnealedO6149   Typ
19   Typ
42   Typ
HardH0482   Typ
74   Typ
4   Typ
SpringH08102   Typ
80   Typ
2   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalConnectorsConductivity (Electrical)Electrical Conductivity
ConnectorsConductivity (Thermal)Thermal Conductivity
ConnectorsMechanical PropertiesModerate Strength
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.