Find suppliers for this alloy
C42210
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | Te(4) | Se(5) | |
|
(1) Cu + Sum of Named Elements 99.7% min. (2) Cu value includes Ag. (3) Includes Co. (4) Te + Se 0.006% max. (5) Te + Se 0.006% max. |
|||||||||
| Min (%) | 86.0 | 1.1 | 0.001 | ||||||
| Max (%) | 89.0 | 0.01 | 1.6 | Rem | 0.035 | 0.010 | 0.5 | 0.005 | 0.005 |
Mechanical Properties
| Melting Point - Liquidus°F | 1905 |
|---|---|
| Melting Point - Solidus°F | 1870 |
| Densitylb/cu in. at 68°F | 0.318 |
| Specific Gravity | 8.8 |
| Electrical Conductivity% IACS at 68°F | 31 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 75 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 10.21 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 18000 |
| Modulus of Rigidityksi | 6700 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Fair |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Excellent |
| Spot Weld | Good |
| Seam Weld | Fair |
| Butt Weld | Good |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Good |
| Machinability Rating | 30 |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications