Find suppliers for this alloyC42210
Chemical Composition
Element
Cu(1,2)PbSnZnFePNi(3)Te(4)Se(5)
(1) Cu + Sum of Named Elements 99.7% min. (2) Cu value includes Ag. (3) Includes Co. (4) Te + Se 0.006% max. (5) Te + Se 0.006% max.
Min (%)86.01.10.001
Max (%)89.00.011.6Rem0.0350.0100.50.0050.005
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Melting Point - Liquidus°F1905
Melting Point - Solidus°F1870
Densitylb/cu in. at 68°F0.318
Specific Gravity8.8
Electrical Conductivity% IACS at 68°F31
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F75
Coefficient of Thermal Expansion 68-21210⁻⁶ per °F (68 – 212°F)10.21
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi18000
Modulus of Rigidityksi6700
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingFair
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingExcellent
Spot WeldGood
Seam WeldFair
Butt WeldGood
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedGood
Machinability Rating30
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialWelded Tube
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.