Find suppliers for this alloyC42230
Chemical Composition
Element
Cu(1)PbSnZnFeCoMnSi
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)87.00.400.300.05
Max (%)91.00.011.5Rem0.051.50.050.30
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Vickers Hardness, 3000 gm
StripHardH0484.1   Min
93.7   Typ
92.3   Max
79.8   Min
82.2   Typ
92.8   Max
197   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1940
Melting Point - Solidus°F1839
Densitylb/cu in. at 68°F0.316
Specific Gravity8.75
Electrical Conductivity% IACS at 68°F34
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F73.2
Modulus of Elasticity in Tensionksi17300
Poisson's Ratio0.345
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingFair
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingNot Recommended
Spot WeldNot Recommended
Seam WeldNot Recommended
Butt WeldGood
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedGood
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalConductors
Terminals Connectors
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.