Find suppliers for this alloy
C42400
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1) | Sn | Zn | Ni | Cr | Si | Zr | |
|
(1) Cu + Sum of Named Elements 99.85% min. |
|||||||
| Min (%) | 87.0 | 0.05 | 0.50 | 0.10 | 0.10 | 0.05 | |
| Max (%) | 91.0 | 0.50 | Rem | 1.5 | 0.50 | 0.30 | 0.20 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Vickers Hardness, 3000 gm |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| Sheet | TM02 |
81.2 Min 85.6 Typ 92.8 Max |
79.8 Min 82.7 Typ |
2 Min |
170 Min 210 Max |
||
| Strip | TM00 |
66.7 Min 74.0 Typ 78.3 Max |
62.4 Min 68.2 Typ |
10 Min |
140 Min 180 Max |
||
| TM01 |
75.4 Min 81.2 Typ 87.0 Max |
72.5 Min 78.3 Typ |
5 Typ |
150 Min 190 Max |
|||
| TM03 |
87.0 Min 91.4 Typ 98.6 Max |
88.5 Typ |
85.6 Typ |
1 Typ |
180 Min 220 Max |
||
Physical Properties
Fabrication Properties
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties