Find suppliers for this alloy
C45450
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Sn | Zn | P | Al | |
| Min (%) | 65.0 | 0.10 | 0.10 | 0.20 | |
| Max (%) | 66.0 | 0.30 | Rem | 0.30 | 0.40 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties