Find suppliers for this alloyC46270
Chemical Composition
Element
Cu(1)PbSnZnFePNiMnSi
(1) Cu + Sum of Named Elements, 99.95% min.
Min (%)62.00.80.6
Max (%)65.00.101.5Rem0.100.200.100.101.2
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Vickers Hardness, 3000 gm
Rod1/2 HardH0282.7   Typ
50.8   Typ
4   Min
175   Typ
As Hot ExtrudedM3072.5   Typ
50.8   Typ
10   Min
150   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1598
Melting Point - Solidus°F1580
Densitylb/cu in. at 68°F0.301
Specific Gravity8.33
Electrical Conductivity% IACS at 68°F14
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingGood
Oxyacetylene WeldingGood
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingGood
Spot WeldNot Recommended
Seam WeldNot Recommended
Butt WeldNot Recommended
Capacity for Being Cold WorkedGood
Capacity for Being Hot FormedExcellent
Forgeability Rating95
Machinability Rating80
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
FastenersScrew Machine Products
PlumbingFittings and valves
Plumbers Fittings
Valve Bodies, Faucets, Plumbing Components
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.