C47200
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | |
| Min (%) | 49.0 | 3.0 | |||
| Max (%) | 52.0 | 0.50 | 4.0 | Rem | 0.10 |