Find suppliers for this alloy
C47940
Elements | ||||||
---|---|---|---|---|---|---|
Cu(1) | Pb | Sn | Zn | Fe | Ni(2) | |
(1) Cu + Sum of Named Elements 99.6% min. (2) Ni value includes Co. |
||||||
Min (%) | 63.0 | 1.0 | 1.2 | 0.10 | 0.10 | |
Max (%) | 66.0 | 2.0 | 2.0 | Rem | 1.0 | 0.50 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
Bar | Navel Brass | ASTM | B21/B21M | NAVAL BRASS ROD, BAR AND SHAPES | |
Rod | Navel Brass | ASTM | B21/B21M | NAVAL BRASS ROD, BAR AND SHAPES | |
Shapes | Navel Brass | ASTM | B21/B21M | NAVAL BRASS ROD, BAR AND SHAPES |
Corrosion Properties