C48600
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | As | |
|
(1) Cu + Sum of Named Elements 99.6% min. |
|||||
| Min (%) | 59.0 | 1.0 | 0.30 | 0.02 | |
| Max (%) | 62.0 | 2.5 | 1.5 | Rem | 0.25 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell B scale | Section Size (in) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| Rod & Wire | 1/2 Hard | H02 |
50 Typ |
25 Typ |
10 Typ |
60 Min 80 Max |
1/2-1 |
| 1/2 Hard | H02 |
40 Typ |
15 Typ |
35 Typ |
35 Min 45 Max |
>2 | |
| 1/2 Hard | H02 |
65 Typ |
30 Typ |
5 Typ |
75 Min 80 Max |
=<1/2 | |
| 1/2 Hard | H02 |
45 Typ |
20 Typ |
20 Typ |
40 Min 75 Max |
1-2 | |
| Soft Anneal | O60 |
40 Typ |
15 Typ |
25 Typ |
40 Min 70 Max |
||
| Melting Point - Liquidus°F | 1645 |
|---|---|
| Melting Point - Solidus°F | 1635 |
| Densitylb/cu in. at 68°F | 0.304 |
| Specific Gravity | 8.42 |
| Electrical Conductivity% IACS at 68°F | 25 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 13 |
| Modulus of Elasticity in Tensionksi | 14600 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Forgings, Die (Hot Pressed) | ASTM | B283/B283M | COPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED) | ||
| ASME | SB283 | COPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED) | |||
| Rod, Bar & Shapes | Forgings | ASTM | B124/B124M | COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES |
Corrosion Properties