Find suppliers for this alloy
C49345
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Bi | Cd | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
|||||||||
| Min (%) | 60.0 | 0.09 | 0.50 | 0.05 | 0.50 | ||||
| Max (%) | 64.0 | 0.25 | 1.5 | Rem | 0.30 | 0.12 | 1.3 | 0.001 | 0.10 |
| Form | Temper | Temper Code | YS-0.5% Ext (ksi) |
Elongation (%) |
Ultimate Tensile Strength in Shear (ksi) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Die Forging | As Hot Forged - Air Cooled | M10 | 20 Min |
20 Min |
50 Min |
| Melting Point - Liquidus°F | 1625 |
|---|---|
| Melting Point - Solidus°F | 1517 |
| Densitylb/cu in. at 68°F | 0.311 |
| Specific Gravity | 8.45 |
| Electrical Conductivity% IACS at 68°F | 19 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 48.7 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 10.8 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 11.2 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11.2 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 14800 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Capacity for Being Cold Worked | Poor |
| Capacity for Being Hot Formed | Good |
| Forgeability Rating | 85 |
| Machinability Rating | 90 |
Common Fabrication Processes
| Treatment | Minimum* | |||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Annealing | 932 | |||
| Hot Working Temperature | 1210 | |||
| Stress Relief | 572 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Automotive | Electrical & Electronic parts | ||
| Plumbing | Enviornmently Friendly Facuets and Plumbing Components |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| ASTM | B967/B967M | COPPER-ZINC-TIN-BISMUTH ALLOY ROD, BAR AND WIRE | |||
| Die Forging | Hot-Pressed | ASTM | B283/B283M | COPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED) | |
| Forgings | ASTM | B124/B124M | COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES | ||
| Forgings, Die (Hot Pressed) | ASME | SB283 | COPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED) | ||
| Rod, Bar & Wire | Free-Cutting | ASTM | B974/B974M | FREE-CUTTING BISMUTH BRASS ROD, BAR AND WIRE |
Corrosion Properties