Find suppliers for this alloy
C49400
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Al | Mg | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||||||
| Min (%) | 57.0 | 0.10 | |||||||||
| Max (%) | 60.0 | 0.10 | 0.30 | Rem | 0.30 | 0.02 | 0.20 | 0.10 | 0.50 | 0.02 | 0.02 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||
| Forgings |
84.1 Typ |
68.2 Typ |
||
| Rod & Bar | As Hot Forged - Air Cooled |
84.1 Typ |
68.2 Typ |
|
| Melting Point - Liquidus°F | 1616 |
|---|---|
| Melting Point - Solidus°F | 1526 |
| Densitylb/cu in. at 68°F | 0.29 |
| Specific Gravity | 7.2 |
| Electrical Conductivity% IACS at 68°F | 24 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11.4 |
| Modulus of Elasticity in Tensionksi | 15200 |
Fabrication Properties
Common Fabrication Processes
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Lead-free,dezincification resistant alloy for potable water components | ||
| Automatic Screw Machine Parts | Lead Free | Machinability, Good |
Applicable Specifications