Find suppliers for this alloy C49450
Chemical Composition
Elements
Cu Pb Sn Zn Fe P Ni Al Mg Mn Si
Min (%) 61.0 0.10
Max (%) 64.0 0.10 0.30 Rem 0.30 0.02 0.20 0.10 0.50 0.10 0.02
Mechanical Properties *
Form Temper Temper Code Tensile Strength
(ksi)
YS-0.2% Offset
(ksi)
* Measured at room temperature, 68°F (20°C).
M10
Forgings As Hot Forged - Air Cooled
Rod & Bar 58.0 Typ
45 Typ
Physical Properties
Densitylb/cu in. at 68°F 0.3
Electrical Conductivity% IACS at 68°F 24
Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Typical Uses

No information for this alloy

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No Corrosion Properties Available.