C50510
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Sn | Zn | P | Ni | |
|
(1) Cu + Sum of Named Elements 99.7% min. |
|||||
| Min (%) | 1.0 | 0.10 | 0.02 | 0.15 | |
| Max (%) | Rem | 1.5 | 0.25 | 0.07 | 0.40 |