Find suppliers for this alloy C50710
Chemical Composition
Elements
Cu(1) Sn P Ni
(1) Cu + Sum of Named Elements 99.5% min.
Min (%) 1.7 0.10
Max (%) Rem 2.3 0.15 0.40
Mechanical Properties *
Form Temper Temper Code Tensile Strength
(ksi)
Elongation
(%)
Vickers Hardness, 3000 gm Section Size
(in)
* Measured at room temperature, 68°F (20°C).
Strip 1/2 Hard H02 59.5 Min
74.0 Max
10 Min
125 Min
165 Max
.10
Annealed O61 45.7 Min
30 Min
70 Min
115 Max
.10
Extra Hard H06 78.3 Min
92.1 Max
2 Min
175 Min
205 Max
.10
Hard H04 71.1 Min
85.6 Max
5 Min
150 Min
185 Max
.10
Spring H08 88.5 Min
102.3 Max
185 Min
.10
Physical Properties
Melting Point - Liquidus°F 1949
Densitylb/cu in. at 68°F 0.318
Specific Gravity 8.88
Electrical Conductivity% IACS at 68°F 32
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F 89.5
Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) 9.81
Specific Heat CapacityBtu/ lb /°F at 68°F 0.089
Modulus of Elasticity in Tensionksi 18100
Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Thermal Properties

No thermal properties for this alloy

Typical Uses

No information for this alloy

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No Corrosion Properties Available.