Find suppliers for this alloyC50780
Chemical Composition
Element
Cu(1)PbSnZnFePNi
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)1.70.050.010.05
Max (%)Rem0.052.30.300.200.350.20
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Flat Products1/2 HardH0265   Typ
51   Typ
10   Typ
1/4 HardH0159   Typ
41   Typ
24   Typ
Extra HardH0690   Typ
86   Typ
5   Typ
HardH0480   Typ
74   Typ
10   Typ
Nominal Grain Size 0.015 mmOS01552   Typ
29   Typ
42   Typ
SpringH0894   Typ
91   Typ
2   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1955
Melting Point - Solidus°F1865
Densitylb/cu in. at 68°F0.32
Specific Gravity8.86
Electrical Conductivity% IACS at 68°F35
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F87
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.9
Modulus of Elasticity in Tensionksi17000
Modulus of Rigidityksi6000
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingFair
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingFair
Spot WeldNot Recommended
Seam WeldNot Recommended
Butt WeldExcellent
Capacity for Being Cold WorkedExcellent
Machinability Rating20
Fabrication Process Properties

No fabrication process properties for this alloy

    
Thermal Properties
Treatment Minimum* Maximum*
* Temperature is measured in Fahrenheit.
Annealing7001350
Typical uses
Product Category Product Reason Category Reason
AutomotiveTerminals, automotiveConductivity (Electrical)Electrical Conductivity
Terminals, automotiveMechanical PropertiesDuctility
Terminals, automotiveMechanical PropertiesStrength
ElectricalConnectors, electronicConductivity (Electrical)Electrical Conductivity
Connectors, electronicCorrosion ResistanceStress Corrosion Crack Resistant
Connectors, electronicMechanical PropertiesStrength, Moderate
Connectors, electronicStress RelaxationStress Relaxation Resistance
Contact springsConductivity (Electrical)Electrical Conductivity
Contact springsCorrosion ResistanceCorrosion Resistance
Contact springsMechanical PropertiesModerate to High Strength
Contact springsSolderabilitySolderability
Lead FramesConductivity (Electrical)Electrical Conductivity
Applicable Specifications
Form Specific Sub-Form System Standard Description
StripElectric Connector & Spring ContactASTMB888/B88MCOPPER ALLOY STRIP FOR USE IN MANUFACTURE OF ELECTRICAL CONNECTORS OR SPRING CONTACTS
Corrosion Properties

No information available.