C50800
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Sn | Fe | P | |
| Min (%) | 2.6 | 0.01 | |||
| Max (%) | Rem | 0.05 | 3.4 | 0.10 | 0.07 |