Find suppliers for this alloy
C51190
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Fe | P | Co | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
||||||
| Min (%) | 3.0 | 0.05 | 0.025 | |||
| Max (%) | Rem | 0.02 | 6.5 | 0.15 | 0.045 | 0.15 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm | Fatigue Strength** (ksi) |
Proportional Limit (ksi) |
Section Size (in) |
|---|---|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | |||||||||
| Flat Products | 1/2 Hard | H02 |
81 Typ |
78 Typ |
16 Typ |
185 Typ |
77 Typ | ||
| Extra Hard | H06 |
100 Typ |
98 Typ |
10 Typ |
228 Typ |
88 Typ | |||
| Hard | H04 |
94 Typ |
92 Typ |
11 Typ |
215 Typ |
39 Typ | 87 Typ | 0.009 | |
| Melting Point - Liquidus°F | 1927 |
|---|---|
| Melting Point - Solidus°F | 1742 |
| Densitylb/cu in. at 68°F | 0.321 |
| Specific Gravity | 8.9 |
| Electrical Conductivity% IACS at 68°F | 22 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 53.2 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 11500 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Fair |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Good |
| Seam Weld | Fair |
| Butt Weld | Excellent |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Good |
| Machinability Rating | 20 |
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Annealing | 842 | |||
| Hot Working Temperature | 1472 | 1742 | ||
| Stress Relief | 523 | |||
Typical Uses
Applicable Specifications
Corrosion Properties