Find suppliers for this alloy
C51800
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | P | Al | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||
| Min (%) | 4.0 | 0.10 | |||
| Max (%) | Rem | 0.02 | 6.0 | 0.35 | 0.01 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Welding Wire | Conductivity (Electrical) | Electrical Conductivity |
| Welding Wire | Conductivity (Thermal) | Thermal Conductivity | |
| Welding Wire | Corrosion Resistance | Oxidation Resistance | |
| Welding Wire | Softening Resistance | Resistance to Thermal Softening |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Electrode | Welding | MILITARY | MIL-E-23765/3 | ELECTRODES, WELDING, BARE, COPPER AND COPPER ALLOY | |
| Rod | Welding | FEDERAL | QQ-R-571 | ROD, WELDING COPPER AND NICKEL ALLOY | |
| Welding | AWS | A5.15 | WELDING RODS FOR WELDING CAST IRON | ||
| Welding | AWS | A5.7 | COPPER AND COPPER ALLOY BARS, WELDING RODS | ||
| Welding | AWS | A5.13 | SURFACE WELDING RODS AND ELECTRODES |
Corrosion Properties