Find suppliers for this alloyC52180
Chemical Composition
Element
Cu(1)PbSnZnFePNi
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)7.00.050.010.05
Max (%)Rem0.059.00.300.200.350.20
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Flat Products1/2 HardH02102   Typ
96   Typ
20   Typ
1/4 HardH0186   Typ
65   Typ
30   Typ
Extra HardH06120   Typ
116   Typ
6   Typ
Extra SpringH10135   Typ
132   Typ
2   Typ
HardH04115   Typ
111   Typ
10   Typ
Nominal Grain Size 0.015 mmOS01569   Typ
34   Typ
51   Typ
SpringH08130   Typ
127   Typ
2   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1880
Melting Point - Solidus°F1620
Densitylb/cu in. at 68°F0.318
Specific Gravity8.8
Electrical Conductivity% IACS at 68°F13
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F36
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)10.1
Modulus of Elasticity in Tensionksi16000
Modulus of Rigidityksi6000
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingFair
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingFair
Spot WeldGood
Seam WeldFair
Butt WeldExcellent
Capacity for Being Cold WorkedGood
Machinability Rating20
Fabrication Process Properties

No fabrication process properties for this alloy

    
Thermal Properties
Treatment Minimum* Maximum*
* Temperature is measured in Fahrenheit.
Annealing7001350
Typical uses
Product Category Product Reason Category Reason
AutomotiveTerminals, automotiveConductivity (Electrical)Electrical Conductivity
Terminals, automotiveMechanical PropertiesDuctility
Terminals, automotiveMechanical PropertiesStrength
ElectricalConnectors, Electrical, Lead-FreeConductivity (Electrical)Electrical Conductivity
Connectors, Electrical, Lead-FreeCorrosion ResistanceStress Corrosion Crack Resistant
Connectors, Electrical, Lead-FreeMechanical PropertiesStrength, Moderate
Connectors, Electrical, Lead-FreeStress RelaxationStress Relaxation Resistance
Contact springsConductivity (Electrical)Electrical Conductivity
Contact springsCorrosion ResistanceCorrosion Resistance
Contact springsMechanical PropertiesModerate to High Strength
Contact springsSolderabilitySolderability
Applicable Specifications
Form Specific Sub-Form System Standard Description
Sheet, Strip, Roller Bar & PlateASTMB103/B103MPHOSPHOR BRONZE PLATE, SHEET, STRIP AND ROLLED BAR
StripElectric Connector & Spring ContactASTMB888/B88MCOPPER ALLOY STRIP FOR USE IN MANUFACTURE OF ELECTRICAL CONNECTORS OR SPRING CONTACTS
Corrosion Properties

No information available.