Find suppliers for this alloy C52850
Chemical Composition
Elements
Cu(1) Sn Al Mn Si
(1) Cu + Sum of Named Elements 99.5% min.
Min (%) 5.0 0.10 0.10
Max (%) Rem 6.0 0.01 0.50 0.50