C53200
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | P | |
| Min (%) | 2.5 | 4.0 | 0.03 | |||
| Max (%) | Rem | 4.0 | 5.5 | 0.20 | 0.10 | 0.35 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.323 |
|---|---|
| Specific Gravity | 8.94 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties