Find suppliers for this alloy
C53800
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Mn | |
|
(1) Cu + Sum of Named Elements 99.8% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
|||||||
| Min (%) | 0.40 | 13.1 | |||||
| Max (%) | Rem | 0.6 | 13.9 | 0.12 | 0.030 | 0.03 | 0.06 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 3000 gm | Section Size (in) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| Rod | Spring | H08 |
131 Min 135 Typ |
116 Min 123 Typ |
1 Min |
260 Typ |
<.100 |
| Spring | H08 |
131 Min 135 Typ |
116 Min 123 Typ |
3 Min |
260 Typ |
<.315 | |
| Wire | Spring | H08 |
138 Min 145 Typ |
123 Min 135 Typ |
3 Min |
280 Typ |
<.100 |
| Spring | H08 |
67 Min 73 Typ |
29 Min 36 Typ |
50 Min |
100 Typ |
<.315 | |
| Melting Point - Liquidus°F | 1796 |
|---|---|
| Melting Point - Solidus°F | 1472 |
| Densitylb/cu in. at 68°F | 0.314 |
| Specific Gravity | 8.7 |
| Electrical Conductivity% IACS at 68°F | 9 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 35 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 10.6 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.086 |
| Modulus of Elasticity in Tensionksi | 12800 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Fair |
| Oxyacetylene Welding | Fair |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Seam Weld | Good |
| Butt Weld | Good |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Poor |
| Forgeability Rating | 20 |
| Machinability Rating | 80 |
Common Fabrication Processes
- Forming
- Machining
| Treatment | Minimum* | Value* | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Stress Relief | 540 | |||
| Annealing | 1200 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Screw Machine Parts | Machining Characteristics | Machinability |
| Spring Contacts | Forming Characteristics | Formability | |
| Spring Contacts | Mechanical Properties | Strength |
Applicable Specifications
Corrosion Properties