Find suppliers for this alloy
C60600
| Elements | |||
|---|---|---|---|
| Cu | Fe | Al | |
| Min (%) | 4.0 | ||
| Max (%) | Rem | 0.50 | 7.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
Torsion Modulus (ksi) |
Fatigue Strength** (ksi) |
Section Size (in) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | |||||||
| Plate | Hard | H04 | 25 Typ |
6.7 Typ | 25 Typ | 0.5 | |
| Soft Anneal | O60 |
45 Typ |
40 Typ |
0.5 | |||
| Densitylb/cu in. at 68°F | 0.295 |
|---|---|
| Specific Gravity | 8.17 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B150/B150M | ALUMINUM BRONZE ROD, BAR AND SHAPES | ||
| Rod | ASTM | B150/B150M | ALUMINUM BRONZE ROD, BAR AND SHAPES | ||
| Shapes | ASTM | B150/B150M | ALUMINUM BRONZE ROD, BAR AND SHAPES |
Corrosion Properties