Find suppliers for this alloyC60600
Chemical Composition
Element
CuFeAl
Min (%)4.0
Max (%)Rem0.507.0
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
Elongation
(%)
Torsion Modulus
(ksi)
Fatigue Strength**
(ksi)
Section Size
(in)
PlateHardH0460  
25   Typ
6.7   Typ
25   Typ
0.5
Soft AnnealO6045   Typ
40   Typ
0.5
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties
Densitylb/cu in. at 68°F0.295
Specific Gravity8.17
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications
Form System Standard Description
BarASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
RodASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
ShapesASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
Corrosion Properties

No information available.