Chemical Composition
Element
Cu(1,2)PbFeAlAs
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag.
Min (%)5.00.02
Max (%)Rem0.100.106.50.35
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell F scale
Torsion Modulus
(ksi)
TubeNominal Grain Size 0.025 mmOS02560   Typ
27   Typ
55   Typ
77   Typ
6.7   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1945
Melting Point - Solidus°F1920
Densitylb/cu in. at 68°F0.295
Specific Gravity8.17
Electrical Conductivity% IACS at 68°F17
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F46
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)10
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi17500
Modulus of Rigidityksi6600
Fabrication Properties
Technique Suitability
SolderingNot Recommended
BrazingFair
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingGood
Spot WeldGood
Seam WeldGood
Butt WeldGood
Capacity for Being Cold WorkedGood
Capacity for Being Hot FormedFair
Machinability Rating20
Common Fabrication Processes
  • Forming and Bending
    
Thermal Properties
Treatment Minimum* Maximum*
* Temperature is measured in Fahrenheit.
Annealing10001200
Hot Treatment14501600
Typical uses
Product Category Product Reason Category Reason
Builders HardwareHardwareAppearanceAppearance
HardwareCorrosion ResistanceCorrosion Resistance
HardwareMechanical PropertiesModerate Strength
FastenersFastenersCorrosion ResistanceCorrosion Resistance
FastenersCorrosion ResistanceCorrosion Resistance in Numerous Environments
FastenersCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
FastenersMechanical PropertiesModerate Strength
IndustrialCondenser TubesCorrosion ResistanceCorrosion Resistance
Condenser TubesCorrosion ResistanceCorrosion Resistance in Numerous Environments
Condenser TubesCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
Condenser TubesForming CharacteristicsFormability
Condenser TubesMechanical PropertiesModerate Strength
Condenser TubesMechanical PropertiesRetains Strength at High Temperatures
Distiller TubesCorrosion ResistanceCorrosion Resistance
Distiller TubesCorrosion ResistanceCorrosion Resistance in Numerous Environments
Distiller TubesCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
Distiller TubesForming CharacteristicsFormability
Distiller TubesMechanical PropertiesModerate Strength
Distiller TubesMechanical PropertiesRetains Strength at High Temperatures
Evaporator TubingCorrosion ResistanceCorrosion Resistance
Evaporator TubingCorrosion ResistanceCorrosion Resistance in Numerous Environments
Evaporator TubingCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
Evaporator TubingForming CharacteristicsFormability
Evaporator TubingMechanical PropertiesRetains Strength at High Temperatures
FerrulesCorrosion ResistanceCorrosion Resistance
FerrulesCorrosion ResistanceCorrosion Resistance in Numerous Environments
FerrulesCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
FerrulesForming CharacteristicsFormability
FerrulesMechanical PropertiesModerate Strength
FerrulesMechanical PropertiesRetains Strength at High Temperatures
Heat Exchanger TubesCorrosion ResistanceCorrosion Resistance
Heat Exchanger TubesCorrosion ResistanceCorrosion Resistance in Numerous Environments
Heat Exchanger TubesCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
Heat Exchanger TubesForming CharacteristicsFormability
Heat Exchanger TubesMechanical PropertiesModerate Strength
Heat Exchanger TubesMechanical PropertiesRetains Strength at High Temperatures
Seamless TubingCorrosion ResistanceCorrosion Resistance
Seamless TubingForming CharacteristicsFormability
Seamless TubingMechanical PropertiesModerate Strength
Structural ComponentsCorrosion ResistanceCorrosion Resistance
Structural ComponentsMechanical PropertiesModerate Strength
Tanks, Corrosion ResistantCorrosion ResistanceCorrosion Resistance
Vessels, Corrosion ResistantCorrosion ResistanceCorrosion Resistance
Vessels, Corrosion ResistantCorrosion ResistanceCorrosion Resistance in Numerous Environments
Vessels, Corrosion ResistantCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
Vessels, Corrosion ResistantMechanical PropertiesModerate Strength
MarineProtective SheathingCorrosion ResistanceCorrosion Resistance
Protective SheathingCorrosion ResistanceCorrosion Resistance in Numerous Environments
Protective SheathingCorrosion ResistanceCorrosion Resistance to Salt Water
Protective SheathingMechanical PropertiesModerate Strength
OrdnanceBlending ChambersCorrosion ResistanceCorrosion Resistance
Blending ChambersMechanical PropertiesModerate Strength
Blending ChambersNon-SparkingNon-Sparking
Mixing TroughsCorrosion ResistanceCorrosion Resistance
Mixing TroughsCorrosion ResistanceCorrosion Resistance in Numerous Environments
Mixing TroughsCorrosion ResistanceCorrosion Resistance to Non Oxidizing Acids
Mixing TroughsMechanical PropertiesModerate Strength
Mixing TroughsNon-SparkingNon-Sparking
Applicable Specifications
Form Application System Standard Description
Seamless Condenser Tube & Ferrule StockCondenser TubeASMESB111COPPER AND COPPER ALLOY SEAMLESS CONDENSER TUBES & FERRULE STOCK
Condenser TubeASTMB111/B111MCOPPER AND COPPER ALLOY SEAMLESS CONDENSER TUBES AND FERRULE STOCK
Seamless Heat Exchanger Tube with Integral FinsASMESB359COPPER & COPPER ALLOY SEAMLESS CONDENSER & HEAT EXCHANGER TUBES WITH INTEGRAL FINS
ASTMB359/B359MCOPPER AND COPPER-ALLOY SEAMLESS CONDENSER AND HEAT EXCHANGER TUBES WITH INTEGRAL FINS
Tubes, Seamless Condenser & Heat Exchanger, U-BendASMESB395U-BEND SEAMLESS COPPER & COPPER ALLOY HEAT EXCHANGER & CONDENSER TUBE
ASTMB395/B395MU-BEND SEAMLESS COPPER AND COPPER ALLOY HEAT EXCHANGER AND CONDENSER TUBES
Corrosion Properties